by dennyhydrostream
Can Nicasil be bored? I was told it couldn't an if so how much to bore a 245 block over 0.15 ?

Re: Honing Nicasil

Posted: Aug 14, 2014 8:44 pm
by rev.ronnie
dennyhydrostream wrote:Can Nicasil be bored? I was told it couldn't an if so how much to bore a 245 block over 0.15 ?
No, it's only around .003" thick. If it needs a bore, it will need to be stripped of the nic, bored, replayed and finish honed. Returning them to standard with a replate is most common.

US Chrome is the most common place to have it done. There are others though.

Re: Honing Nicasil

Posted: Aug 14, 2014 9:36 pm
by dennyhydrostream
ok thanks for the info

Re: Honing Nicasil

Posted: Aug 14, 2014 11:13 pm
by rev.ronnie
Replated that is. Damn spellcheck.